X38CrMoV5-3
Chemical Composition (%) | C | Si | Mn | Cr | Mo | V |
% Average | 0,38 | 0,40 | 0,40 | 2,95 | 2,75 | 0,55 |
DIN Analysis | 0,35-0,40 | 0,30-0,50 | 0,30-0,50 | 4,80-5,20 | 2,70-3,20 | 0,40-0,60 |
Thermal Conductivity ( W/ m.K ) | 20°C | 350°C | 700°C |
36,4 | 32,2 | 27,5 |
HEAT TREATMENT | |||
Tempature(°C) | Time (Hour) | Cooling Environment | |
Soft Annealing | 800-840 | 2-5* | Furnace |
Stress Relief Annealing | 600-650 | 2* | Furnace |
Hardening | 1030-1060 | - | Air, Oil, Hot bath 500-550°C |
Tempering | 540-700 | 1 hour for every 20 mm | Air |