90MnCrV8 / AISI: O2
Chemical Composition (%) | C | Si | Mn | Cr | V |
% Average | 0,90 | 0,25 | 2,00 | 0,35 | 0,10 |
DIN Analysis | 0,85-0,95 | 0,10-0,40 | 1,80-2,20 | 0,20-0,50 | 0,05-0,20 |
Thermal Conductivity ( W/ m.K ) | 20°C | 350°C | 700°C |
33,0 | 32,0 | 31,3 |
HEAT TREATMENT | |||
Tempature(°C) | Time (Hour) | Cooling Environment | |
Soft Annealing | 680-720 | 2-5* | Furnace |
Stress Relief Annealing | 600-650 | 2* | Furnace |
Hardening | 790-820 | - | Yağ, 180-220°C |
Tempering | 180-300 | 1 hour for every 20 mm | Air |